Case studies · Industrial pilot
Measuring from below through a controlled water layer
In an environment full of chips, dust and lubricants, mechanical contact between an ultrasonic probe and metal scratches the surface and makes the signal drift. Changing the beam entry direction and using a trough module solved the problem.
Challenge
The client required continuous detection of defects at the edges of 3 mm steel strips/sheets moving at 1 m/s. Probes with a hard delay line failed: mechanical pressure scratched the sheet, and chips and grease on the top surface caused unstable acoustic coupling.
OPTEL solution
- Inverted measuring geometry: probes placed under the clean bottom surface of the sheet, away from chips lying on top.
- Two-chamber overflow trough: instead of hard contact, a controlled liquid column with a soft PTFE seal and forced water circulation.
- Precise beam refraction (10.5° → 45°): a longitudinal wave incident in water at about 10.5° is refracted to about 45° in steel and penetrates the edge zone.
- Advanced signal processing: time of flight (TOF), envelope and correlation analysis with continuous compensation of sound velocity vs. liquid temperature.
Results
- Zero surface damage: no friction or scratching of the sheet at 1 m/s.
- Stable measurement: immune to process contamination and ambient temperature changes.
Key parameters
- Material: steel sheet/strip 3 mm
- Feed speed: 1 m/s
- Beam: longitudinal wave ~10.5° in water → ~45° in steel
- Coupling: two-chamber water trough with PTFE seal
Related pages
Facing an unusual measurement problem in harsh industrial conditions? We will design an acoustic path tailored to your line.
Custom ultrasonic development
Need a solution for a specific measurement problem?
OPTEL can evaluate the measurement physics, transducers, electronics and software before a full system is built.
Start with a feasibility studyContact OPTEL